Material Characterization and Test Specimens
Material representativeness in additive manufacturing
In additive manufacturing, mechanical properties depend on the build orientation (anisotropy) and on the machine parameters. A supplier datasheet is not enough to validate an aerospace or medical part. Initial produces batches of test specimens (tensile, flexural, impact) printed with exactly the same parameters (laser, temperature, orientation) as your future production parts.
- Process qualification confirms that the machine holds the target tolerances.
- Material qualification measures the Young’s modulus, the stress at break or the fire behaviour on one specific powder batch.
- Technology benchmarking means printing the same specimen in SLS, in MJF and in injection molding, so the best technology is chosen on factual grounds.
These tests complement the validation carried out on functional prototypes: the standard specimen isolates the material data, the real part validates the geometry.
Standards and specifications
We produce test specimens that comply with international standards for your test benches:
Testing and traceability
Beyond printing, we run the tests and supply a complete characterization report. Dimensional inspection is based on a 3D scan report of the specimen, density is verified by weighing, and traceability is ensured through a material certificate (virgin or recycled powder) and a machine batch number.
Beyond mechanical testing
Characterization is not limited to tensile and flexural testing. Compression (ISO 604) measures how the material behaves under crushing loads, which matters for structural parts and supports. Temperature resistance is qualified through the heat deflection temperature, or HDT (ISO 75), a decisive criterion for under-bonnet applications or locations close to a heat source. Density (ISO 1183) checks the specific gravity and, indirectly, the internal porosity of a powder batch. These measurements complete the material profile and secure the move to production.
What a characterization report contains
An Initial characterization report brings together the stress-strain curves of each test, the key values (Young’s modulus, stress and elongation at break), the dimensional inspection of the specimen, the density measurement and the full traceability of the batch: material, machine, parameters and build orientation. This document feeds your qualification file and allows two materials or two technologies to be compared objectively, on figures.
What about metal parts?
Material characterization does not stop at polymers. A 3D printed metal part requires the same qualification work: specimens produced under the same conditions as the part, and tests carried out to the applicable standards. Our feature on testing and characterising metal 3D printing details the processes and alloys available.
Frequently asked questions
To characterize anisotropy. We often print specimens flat (XY) and upright (Z) to measure the difference in properties between layers (in Z).
We have a library of STL files compliant with ISO and ASTM standards. We can also print your own specimen designs (fatigue specimens, tubular specimens).
We recommend testing the material targeted for production. PA12 (polyamide) is the standard choice, but we also characterize PA11, PP01 and PA3200 GF (glass filled).
Standards generally recommend at least five specimens per condition to obtain a representative mean and standard deviation. We adjust that number to the confidence level required and to the demands of the sector, which are higher in aerospace and medical applications.